Oxidation resistance of Ti 3 AlC 2 and Ti 3 Al 0.8 Sn 0.2 C 2 MAX phases: A comparison

2019

Ti3AlC2 and Ti3Al0.8Sn0.2C2 MAX phase powders are densified using Spark Plasma Sintering technique to obtain dense bulk materials. Oxidation tests are then performed over the temperature range 800-1000°C under synthetic air on the two different materials in order to compare their oxidation resistance. It is demonstrated that, in the case of the Ti3Al0.8Sn0.2C2 solid solution, the oxide layers consist in TiO2, Al2O3 and SnO2. The presence of Sn atoms in

010302 applied physicsMaterials scienceOxideAnalytical chemistrySpark plasma sintering02 engineering and technologyAtmospheric temperature range021001 nanoscience & nanotechnology01 natural sciences3. Good healthchemistry.chemical_compoundchemistryPhase (matter)0103 physical sciencesMaterials ChemistryCeramics and CompositesMAX phases0210 nano-technologyOxidation resistanceSolid solutionJournal of the American Ceramic Society